TIG / MIG ERNiCrMo-4 Hastelloy C276 Kawat las

Rincian produk

/haynes-25-alloy-l605-co350-las-kawat-produk/

ErNiCrMo-4 Hastelloy C276(UNS 10276) Kawat las

Ngaran Bahan las: Kawat Las Nikel, Kawat Las ErNiCrMo-4, Kawat Las Hastelloy C276

♦ MOQ: 15 kg

♦ Bentuk: MIG(15kgs/spool), TIG(5kgs/box)

♦ Ukuran: Diaméterna 0.01mm-8.0mm

♦ Ukuran umumUkuran: 0.8MM / 1.0MM / 1.2MM / 1.6MM / 2.4MM / 3.2MM / 3.8MM / 4.0MM / 5.0MM

♦ Standar: Conforms kana Sertifikasi AWS A5.14 ASME SFA A5.14

 ErNiCrMo-4 dipaké pikeun las Hastelloy C276, alloy base nikel jeung bahan séjén, alloy nikel kana baja atawa stainless steel, ogé dipaké pikeun las nikel CrMo alloy lapisan komposit dina steel.Main bahan las komposisi kimia sarupa kitu ogé bahan dissimilar tina alloy base nikel. , steels sarta stainless steels.alloy ieu ogé bisa dipaké pikeun cladding baja jeung nikel-chrome-molybdenum weld logam.Eusi molybdenum nu leuwih luhur nyadiakeun résistansi hébat kana stress korosi cracking, pitting na crevice korosi.

Komposisi Kimia ERNiCrMo-4

C

Cr

Ni

Si

Mn

P

S

Cu

Fe

V

W

Mo

Co

≤0.02

14.5-16.5

Ba ≤0.08 ≤1.0 ≤0.04 ≤0.03 ≤0.5 4.0-7.0

≤0.35

3.0-4.0 15.0-17.0 ≤2.5
ERNiCrMo-4 Paraméter las has
Diameter Prosés Volt Amp Gas pelindung
In mm
0.035 0.9 GMAW 26-29 150-190 Semprot Transfer100% Argon
0.045 1.2 GMAW 28-32 180-220
1/16 1.6 GMAW 29-33 200-250
1/16 1.6 GMAW 14-18 90-130 100% Argon
3/32 2.4 GMAW 15-20 120-175 100% Argon
1/8 3.2 GMAW 15-20 150-220 100% Argon
ERNiCrMo-4 Sipat mékanis

 

Kaayaan Kakuatan Tensile MPa (ksi) Kakuatan ngahasilkeun MPa (ksi) Elongation%
AWS reauirement 690(100) Henteu ditangtoskeun Henteu ditangtoskeun
Hasilna has salaku dilas 730(106) 540(79) 39

GAS TAPI:

MIG: 75% Ar / 25% Anjeunna

TIG: 100% Ar

Naha ERNiCrMo-4?

 alloy nu tahan ka asam sarta uap asam corrosion.Because eusi molybdenum tinggi na, éta boga daya tahan kuat ka stress retakan korosi, pitting na cavitation korosi.

ERNiCrMo-4Widang aplikasi:

Loba dipaké dina pipelines wadahna kimiawi, valves pompa, industri kakuatan flue gas desulfurization na las -196 ℃ aplikasi tina 9% Ni baja.